Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.70 | 0.80 | ||
Si | 1.25 | 1.75 | ||
Mn | 0.40 | 0.70 | ||
P | - | 0.035 | ||
S | - | 0.030 | ||
Cr | 19.00 | 21.00 | ||
Ni | - | - | ||
Mo | 1.40 | 1.80 |
Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
596 (≥) | 225 (≥) | 13 | 31 | 42 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 423 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
319 (≥) | 952 (≥) | 31 | 31 | 24 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 334 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
668 | 228 | 645 |
We can customize the production of 80X20HC grade, contact us for the best solution.