A 493 S42010 Stainless Steels to A 493 (2009)

A 493 S42010 - Specification & Application

  • A 493 (2009) - Stainless Steel Wire and Wire Rods for Cold Heading and Cold Forging

Stainless Steel Wire and Wire Rods for Cold Heading and Cold Forging

Chemical composition(wt.%) of A 493 S42010 grade: to A 493 (2009)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.15 0.30
Mn - 1.00
Si - 1.00
P - 0.04
S - 0.03
Cr 13.50 15.00
Ni 0.25 1.00
Mo 0.40 1.00

A 493 S42010 - Detail

Stainless Steel Wire and Wire Rods for Cold Heading and Cold Forging

Mechanical properties of grade A 493 S42010 A 493 (2009)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
224 (≥) 246 (≥) 42 43 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 234

Physical properties of grade A 493 S42010 A 493 (2009)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
988 (≥) 933 (≥) 41 22 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 344
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
952 664 375

Equivalent Products

We can customize the production of A 493 S42010 grade, contact us for the best solution.
sales@specificsteel.com