In 00cr19ni10 adding N, on the basis of the above grades also features, use the same as the 0 cr19ni9n, but better intergranular corrosion resistance
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.030 | ||
Si | - | 1.00 | ||
Mn | - | 2.00 | ||
P | - | 0.035 | ||
S | - | 0.030 | ||
Ni | 8.50 | 11.50 | ||
Cr | 17.00 | 19.00 | ||
N | 0.12 | 0.22 |
00Cr18Ni10N
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
873 (≥) | 343 (≥) | 11 | 24 | 24 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 141 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
159 (≥) | 949 (≥) | 24 | 44 | 33 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 214 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
163 | 864 | 127 |
We can customize the production of 00Cr18Ni10N grade, contact us for the best solution.