Alloyed CrMo steel
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.90 | 1.10 | ||
Si | 0.15 | 0.30 | ||
Mn | 0.20 | 0.40 | ||
P | - | 0.035 | ||
S | - | 0.035 | ||
Cr | 1.10 | 1.30 | ||
Mo | 0.20 | 0.40 | ||
V | - | - |
Alloyed CrMo steel
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
279 (≥) | 345 (≥) | 12 | 32 | 43 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 422 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
817 (≥) | 732 (≥) | 24 | 32 | 43 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 212 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
644 | 486 | 438 |
We can customize the production of 1.2203 grade, contact us for the best solution.
–sales@specificsteel.com