Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.17 | 0.25 | ||
Si | - | 0.80 | ||
Mn | - | 0.80 | ||
P | - | 0.035 | ||
S | - | 0.025 | ||
Cr | 16.00 | 18.00 | ||
Ni | 1.50 | 2.50 | ||
Mo | - | 0.30 | ||
W | - | 0.20 | ||
Ti | - | 0.20 |
Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
247 (≥) | 528 (≥) | 23 | 31 | 33 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 231 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
496 (≥) | 636 (≥) | 23 | 33 | 21 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 322 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
411 | 428 | 874 |
We can customize the production of 20X17H2 grade, contact us for the best solution.