A 269 S34565 Stainless Steels to A 269 (2010)

A 269 S34565 - Specification & Application

  • A 269 (2010) - Seamless and Welded Austenitic Stainless Steel Tubing for General Service

Seamless and Welded Austenitic Stainless Steel Tubing for General Service

Chemical composition(wt.%) of A 269 S34565 grade: to A 269 (2010)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Mn 5.00 7.00
Si - 1.00
P - 0.03
S - 0.01
Cr 23.00 25.00
Ni 16.00 18.00
Mo 4.00 5.00
N 0.40 0.60
Nb - 0.10

A 269 S34565 - Detail

Seamless and Welded Austenitic Stainless Steel Tubing for General Service

Mechanical properties of grade A 269 S34565 A 269 (2010)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
685 (≥) 117 (≥) 31 43 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 423

Physical properties of grade A 269 S34565 A 269 (2010)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
376 (≥) 946 (≥) 44 31 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 331
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
127 395 933