Welded Austenitic Steel Boiler, Superheater, Heat-Exchanger, and Condenser Tubes
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.08 | ||
Si | - | 1.00 | ||
Mn | 11.5 | 14.5 | ||
P | - | 0.06 | ||
S | - | 0.03 | ||
Cr | 17.0 | 19.0 | ||
Ni | 2.25 | 3.75 | ||
N | 0.20 | 0.40 |
A 269 TPXM-29
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
164 (≥) | 836 (≥) | 13 | 12 | 14 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 344 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
822 (≥) | 717 (≥) | 24 | 31 | 23 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 431 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
955 | 158 | 676 |
We can customize the production of A 269 TPXM-29 grade, contact us for the best solution.