Iron-based superalloy
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.02 | 0.06 | ||
Cr | 11.0 | 14.0 | ||
Mo | 5.0 | 6.5 | ||
Ni | 40.0 | 45.0 | ||
Al | - | 0.3 | ||
Ti | 2.8 | 3.1 | ||
B | 0.001 | 0.02 | ||
Mn | - | 0.4 | ||
Fe | - | Remainder |
GH2901
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
276 (≥) | 237 (≥) | 42 | 34 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 423 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
516 (≥) | 977 (≥) | 34 | 21 | 42 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 113 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
774 | 847 | 386 |
We can customize the production of GH2901 grade, contact us for the best solution.
–sales@specificsteel.com