Nickel-base superalloy
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.08 | ||
Cr | 13.0 | 16.0 | ||
Mo | 2.8 | 3.2 | ||
Ni | - | Remainder | ||
Al | 1.3 | 1.7 | ||
Nb | 1.8 | 2.2 | ||
Ti | 2.35 | 2.75 | ||
B | - | 0.005 | ||
Fe | - | 2.0 | ||
Ce | - | 0.005 |
GH4698
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
272 (≥) | 934 (≥) | 12 | 31 | 14 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 414 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
395 (≥) | 499 (≥) | 32 | 11 | 21 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 133 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
483 | 856 | 994 |
We can customize the production of GH4698 grade, contact us for the best solution.