Nickel-base superalloy
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.02 | 0.07 | ||
Cr | 12.0 | 14.0 | ||
Mo | 1.4 | 1.9 | ||
Ni | 42.0 | 45.0 | ||
W | 2.8 | 3.2 | ||
Al | 1.4 | 1.85 | ||
Ti | 3.15 | 3.65 | ||
B | - | 0.01 | ||
Ce | - | 0.03 |
GH4761
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
672 (≥) | 315 (≥) | 32 | 24 | 31 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 421 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
982 (≥) | 812 (≥) | 12 | 43 | 24 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 141 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
556 | 411 | 353 |
We can customize the production of GH4761 grade, contact us for the best solution.
–sales@specificsteel.com