Heat-resistant steels
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.12 | ||
Si | 0.70 | 1.40 | ||
Mn | - | 1.00 | ||
P | - | 0.040 | ||
S | - | 0.030 | ||
Cr | 17.00 | 19.00 | ||
Ni | - | 1.00 | ||
Al | 0.70 | 1.20 |
Heat-resistant steels
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
737 (≥) | 575 (≥) | 31 | 42 | 41 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 124 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
689 (≥) | 296 (≥) | 44 | 24 | 14 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 422 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
551 | 239 | 758 |
We can customize the production of ISO H5 grade, contact us for the best solution.
–sales@specificsteel.com