NiCr15Fe Stainless Steels to BS EN 10095

NiCr15Fe - Specification & Application

  • BS EN 10095 - Heat resisting steels and nickel alloys

Heat resisting steels and nickel alloys

Chemical composition(wt.%) of NiCr15Fe grade: to BS EN 10095

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.05 0.10
Si - 0.50
Mn - 1.00
P - 0.020
S - 0.015
Cr 14.00 17.00
Ni 72.00 -
Al - 0.30
Ti - 0.30
Fe 6.00 10.00
Cu - 0.30

NiCr15Fe - Detail

Heat resisting steels and nickel alloys

Mechanical properties of grade NiCr15Fe BS EN 10095

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
114 (≥) 317 (≥) 11 32 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 341

Physical properties of grade NiCr15Fe BS EN 10095

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
365 (≥) 371 (≥) 14 42 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 343
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
466 275 424

Equivalent Products