Nickel Alloy, Corrosion and Heat Resistant, Sheet, Strip, and Plate 45.5Ni - 25.5Cr - 3.2Co - 3.2Mo - 3.2W - 18.5Fe Solution Heat Treated
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.04 | ||
Si | - | 1.15 | ||
Mn | - | 1.00 | ||
Cr | - | 25.50 | ||
Ni | - | remaining | ||
Mo | - | 3.25 | ||
Co | - | 3.00 | ||
W | - | 3.25 | ||
Al | - | - | ||
Cu | - | 0.10 | ||
Ti | - | - | ||
Fe | - | 17.00 |
Nickel Alloy, Corrosion and Heat Resistant, Sheet, Strip, and Plate 45.5Ni - 25.5Cr - 3.2Co - 3.2Mo - 3.2W - 18.5Fe Solution Heat Treated
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
774 (≥) | 599 (≥) | 22 | 22 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 321 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
741 (≥) | 227 (≥) | 13 | 24 | 13 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 313 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
833 | 564 | 252 |