S.205 Stainless Steels to BS S 205

S.205 - Specification & Application

  • BS S 205 - Specification for austenitic chromium-nickel steel wire and springs

Specification for austenitic chromium-nickel steel wire and springs

Chemical composition(wt.%) of S.205 grade: to BS S 205

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Si 0.20 1.00
Mn 0.50 2.00
P - 0.035
S - 0.025
Cr 17.00 19.00
Ni 7.50 9.00
Mo - -
Nb/Ti - -

S.205 - Detail

Specification for austenitic chromium-nickel steel wire and springs

Mechanical properties of grade S.205 BS S 205

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
949 (≥) 614 (≥) 12 43 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 333

Physical properties of grade S.205 BS S 205

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
717 (≥) 368 (≥) 12 12 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 434
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
544 734 733

Equivalent Grade

Equivalent Products

We can customize the production of S.205 grade, contact us for the best solution.