Martensitic Chromium Stainless Steel
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.15 | ||
Mn | - | 1.25 | ||
Si | - | 1.00 | ||
P | - | 0.06 | ||
S | - | 0.15 | ||
Cr | 12.00 | 14.00 | ||
Ni | - | - | ||
Mo | - | 0.60 |
Martensitic Chromium Stainless Steel
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
497 (≥) | 398 (≥) | 24 | 23 | 22 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 314 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
963 (≥) | 656 (≥) | 41 | 21 | 14 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 143 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
555 | 922 | 777 |
We can customize the production of S42020 grade, contact us for the best solution.
–sales@specificsteel.com