SUS 303Cu Stainless Steels to G 4303 (2005)

SUS 303Cu - Specification & Application

  • G 4303 (2005) - Stainless steel bars
  • G 4308 (2007) - Stainless steel wire rods
  • G 4309 (1999) - Stainless steel wires
  • G 4318 (2007) - Cold finished stainless steel bars

Austenitic stainless steel; B (bars) can be suffixed to the symbol of the grade; Round bars, square bars, hexagonal bars and flat bars, hereafter generically reffered to as "bars".

Chemical composition(wt.%) of SUS 303Cu grade: to G 4303 (2005)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Si - 1.00
Mn - 2.00
P - 0.15
S 0.10 -
Cr 17.0 19.0
Ni 6.00 10.0
Cu 2.50 4.00
Se 0.10 -

SUS 303Cu - Detail

Austenitic stainless steel; B (bars) can be suffixed to the symbol of the grade; Round bars, square bars, hexagonal bars and flat bars, hereafter generically reffered to as "bars".

Mechanical properties of grade SUS 303Cu G 4303 (2005)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
885 (≥) 468 (≥) 32 44 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 442

Physical properties of grade SUS 303Cu G 4303 (2005)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
671 (≥) 551 (≥) 34 31 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 244
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
851 131 432

Equivalent Products

We can customize the production of SUS 303Cu grade, contact us for the best solution.
sales@specificsteel.com