Heat-resistant steels
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.15 | ||
Si | 1.00 | 2.00 | ||
Mn | - | 2.00 | ||
P | - | 0.045 | ||
S | - | 0.030 | ||
Cr | 15.00 | 17.00 | ||
Ni | 33.00 | 37.00 |
Heat-resistant steels
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
577 (≥) | 656 (≥) | 31 | 43 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 311 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
877 (≥) | 136 (≥) | 24 | 34 | 21 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 423 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
436 | 554 | 112 |
We can customize the production of X12NiCrSi35-16 grade, contact us for the best solution.