X4CrNiMo16-5-1 Stainless Steels to NF EN 10028-7

X4CrNiMo16-5-1 - Specification & Application

  • NF EN 10028-7 - Flat products made of steels for pressure purposes - Part 7: Stainless steels
  • NF EN 10088-1 - Stainless steels - Part 1: List of stainless steels
  • NF EN 10088-2 - Stainless steels - Part 2: Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for general purposes
  • NF EN 10088-3 - Stainless steels - Part 3: Technical delivery conditions for semi-finished products, bars, rods, wire, sections and bright products of corrosion resisting steels for general purposes
  • NF EN 10088-4 - Stainless steels - Part 4: Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for construction purposes
  • NF EN 10088-5 - Stainless steels - Part 5: Technical delivery conditions for bars, rods, wire, sections and bright products of corrosion resisting steels for construction purposes
  • NF EN 10250-4 - Open die steel forgings for general engineering purposes - Part 4: Stainless steels
  • NF EN 10272 - Stainless steel bars for pressure purposes
  • NF EN 4629 - Aerospace series - Steel FE-PM 3504 (X4CrNiMo16-5-1) - Air melted - Hardened and tempered - Forging stock - De = 300 mm
  • NF EN 4631 - Aerospace series - Steel FE-PM 3504 (X4CrNiMo16-5-1) - Air melted - Hardened and tempered - Bar - De = 200 mm - 900 MPa = Rm = 1 050 MPa

Aerospace series - Steel FE-PM 3504 (X4CrNiMo16-5-1) - Air melted - Hardened and tempered - Bar - De = 200 mm - 900 MPa = Rm = 1 050 MPa

Chemical composition(wt.%) of X4CrNiMo16-5-1 grade: to NF EN 10028-7

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.06
Si - 0.70
Mn - 1.50
P - 0.040
S - 0.015
Cr 15.00 17.00
Mo 0.80 1.50
Ni 4.00 6.00
N 0.020 -

X4CrNiMo16-5-1 - Detail

Aerospace series - Steel FE-PM 3504 (X4CrNiMo16-5-1) - Air melted - Hardened and tempered - Bar - De = 200 mm - 900 MPa = Rm = 1 050 MPa

Mechanical properties of grade X4CrNiMo16-5-1 NF EN 10028-7

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
349 (≥) 728 (≥) 11 11 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 432

Physical properties of grade X4CrNiMo16-5-1 NF EN 10028-7

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
237 (≥) 797 (≥) 34 11 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 112
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
491 357 376

Equivalent Products

We can customize the production of X4CrNiMo16-5-1 grade, contact us for the best solution.