Heat-resistant steels
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.08 | ||
Si | 0.75 | 1.50 | ||
Mn | - | 2.00 | ||
P | - | 0.030 | ||
S | - | 0.030 | ||
Cr | 17.00 | 20.00 | ||
Ni | 34.00 | 37.00 | ||
Cu | - | 1.00 | ||
Pb | - | 0.005 | ||
Sn | - | 0.025 |
Heat-resistant steels
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
787 (≥) | 954 (≥) | 44 | 44 | 13 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 242 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
133 (≥) | 267 (≥) | 42 | 21 | 33 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 223 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
917 | 786 | 557 |
We can customize the production of X6NiCrSi36-19 grade, contact us for the best solution.