Z3CNDU22-07Az Stainless Steels to NF A 35-578

Z3CNDU22-07Az - Specification & Application

  • NF A 35-578 - Iron and steel. Stainless steel for high temperature application
  • NF A 36-209 - Iron and steel. Austenitic and austenic-ferritic stainless steels plates for boilers and pressure vessels
  • NF A 49-244 - Steel tubes - Welded austenitic stainless and austenitic ferritic steel rolled tubes for pressure service - Dimensions, technical conditions for delivery

Steel tubes - Welded austenitic stainless and austenitic ferritic steel rolled tubes for pressure service - Dimensions, technical conditions for delivery

Chemical composition(wt.%) of Z3CNDU22-07Az grade: to NF A 35-578

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 0.75
Mn - 2.00
P - 0.035
S - 0.010
Cr 21.00 23.00
Mo 2.70 3.90
Ni 5.50 7.50
Cu 1.00 2.00
N 0.05 0.19

Z3CNDU22-07Az - Detail

Steel tubes - Welded austenitic stainless and austenitic ferritic steel rolled tubes for pressure service - Dimensions, technical conditions for delivery

Mechanical properties of grade Z3CNDU22-07Az NF A 35-578

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
588 (≥) 164 (≥) 23 33 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 341

Physical properties of grade Z3CNDU22-07Az NF A 35-578

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
934 (≥) 112 (≥) 12 43 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 241
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
444 399 129

Equivalent Products

We can customize the production of Z3CNDU22-07Az grade, contact us for the best solution.
sales@specificsteel.com