Iron and steel. Stainless steel wire rods for cold forming
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.020 | 0.050 | ||
Si | 0.50 | 1.00 | ||
Mn | 1.00 | 1.50 | ||
P | - | 0.040 | ||
S | - | 0.010 | ||
Cr | 16.50 | 17.50 | ||
Mo | 2.00 | 2.50 | ||
Ni | 10.50 | 11.50 |
Iron and steel. Stainless steel wire rods for cold forming
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
127 (≥) | 675 (≥) | 23 | 33 | 41 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 314 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
535 (≥) | 564 (≥) | 23 | 44 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 212 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
991 | 122 | 657 |
We can customize the production of Z4CND17-11-02FF grade, contact us for the best solution.
–sales@specificsteel.com