KSUS304N2 Stainless Steels

KSUS304N2 - Specification & Application

Rolled Stainless Steels

Chemical composition(wt.%) of KSUS304N2 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn - 2.50
P - 0.045
S - 0.03
Cr 18.00 20.00
Ni 7.50 10.50
Mo - -
N 0.15 0.30
Nb - 0.15

KSUS304N2 - Detail

Rolled Stainless Steels

Mechanical properties of grade KSUS304N2

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
859 (≥) 926 (≥) 43 44 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 122

Physical properties of grade KSUS304N2

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
572 (≥) 794 (≥) 24 22 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 322
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
756 156 826

Equivalent Products

We can customize the production of KSUS304N2 grade, contact us for the best solution.