Specification for nickel and nickel alloys: bar
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.15 | ||
Si | - | 0.35 | ||
Mn | - | 0.35 | ||
P | - | - | ||
S | - | 0.010 | ||
Cr | - | - | ||
Ni | 99.00 | - | ||
Mo | - | - | ||
Al | - | - | ||
Cu | - | 0.25 | ||
Ti | - | 0.10 | ||
Fe | - | 0.40 | ||
Mg | - | 0.20 |
Specification for nickel and nickel alloys: bar
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
689 (≥) | 172 (≥) | 31 | 41 | 43 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 341 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
486 (≥) | 395 (≥) | 44 | 21 | 24 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 212 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
944 | 268 | 189 |
We can customize the production of NA11 grade, contact us for the best solution.