NCF751 Stainless Steels

NCF751 - Specification & Application

CNS Standard heat resistant alloy and corrosion resistant alloy bar and plate type and chemical composition

Chemical composition(wt.%) of NCF751 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.10
Si - 0.50
Mn - 1.00
P - 0.030
S - 0.015
Cr 14.00 17.00
Ni 70.00 -
Cu - 0.50
Al 0.90 1.50
Ti 2.00 2.60
Fe 5.00 9.00

NCF751 - Detail

CNS Standard heat resistant alloy and corrosion resistant alloy bar and plate type and chemical composition

Mechanical properties of grade NCF751

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
445 (≥) 457 (≥) 32 42 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 243

Physical properties of grade NCF751

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
737 (≥) 244 (≥) 14 22 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 314
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
694 981 986

Equivalent Products

We can customize the production of NCF751 grade, contact us for the best solution.