Chemical composition(wt.%) of STS630FB grade: to D 3691 (2001)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.07
Si - 1.00
Mn - 1.00
P - 0.040
S - 0.030
Cr 15.00 17.00
Ni 3.00 5.00
Mo - -
N - -
Cu 3.00 5.00
Nb 0.15 0.45

STS630FB - Detail

Stainless steel blooms and billets for forgings

Mechanical properties of grade STS630FB D 3691 (2001)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
642 (≥) 789 (≥) 44 22 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 221

Physical properties of grade STS630FB D 3691 (2001)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
644 (≥) 277 (≥) 22 21 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 433
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
266 471 243