CNS standard heat resistant steel bar steel grade and chemical composition
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.45 | 0.55 | ||
Si | - | 1.00 | ||
Mn | - | 2.00 | ||
P | - | 0.030 | ||
S | - | 0.030 | ||
Cr | 7.50 | 9.50 | ||
Ni | - | 0.60 | ||
Mo | - | - | ||
N | - | - |
CNS standard heat resistant steel bar steel grade and chemical composition
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
286 (≥) | 263 (≥) | 41 | 33 | 34 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 224 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
734 (≥) | 954 (≥) | 43 | 42 | 24 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 242 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
424 | 788 | 389 |
We can customize the production of SUH11 grade, contact us for the best solution.
–sales@specificsteel.com