SUH37 Stainless Steels

SUH37 - Specification & Application

CNS standard heat resistant steel bar steel grade and chemical composition

Chemical composition(wt.%) of SUH37 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.15 0.25
Si - 1.00
Mn 1.00 1.60
P - 0.040
S - 0.030
Cr 20.50 22.50
Ni 10.00 12.00
Mo - -
N 0.15 0.30

SUH37 - Detail

CNS standard heat resistant steel bar steel grade and chemical composition

Mechanical properties of grade SUH37

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
728 (≥) 758 (≥) 31 12 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 114

Physical properties of grade SUH37

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
674 (≥) 485 (≥) 32 32 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 232
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
992 458 491

Equivalent Grade

Equivalent Products

We can customize the production of SUH37 grade, contact us for the best solution.
sales@specificsteel.com