SUS 304 LTP Stainless Steels to G 3459 (2012)

SUS 304 LTP - Specification & Application

  • G 3459 (2012) - Stainless steel pipes

Stainless steel pipes

Chemical composition(wt.%) of SUS 304 LTP grade: to G 3459 (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.03
Cr 18.00 20.00
Ni 9.00 13.00
Mo - -
N - -

SUS 304 LTP - Detail

Stainless steel pipes

Mechanical properties of grade SUS 304 LTP G 3459 (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
396 (≥) 693 (≥) 11 42 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 111

Physical properties of grade SUS 304 LTP G 3459 (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
971 (≥) 884 (≥) 22 42 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 342
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
697 175 893