SUS 304N1-WPA Stainless Steels to G 4314 (1994)

SUS 304N1-WPA - Specification & Application

  • G 4314 (1994) - Stainless steel wires for springs

Stainless steel wires for springs

Chemical composition(wt.%) of SUS 304N1-WPA grade: to G 4314 (1994)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn - 2.50
P - 0.045
S - 0.03
Cr 18.00 20.00
Ni 7.00 10.50
Mo - -
N 0.10 0.25

SUS 304N1-WPA - Detail

Stainless steel wires for springs

Mechanical properties of grade SUS 304N1-WPA G 4314 (1994)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
865 (≥) 538 (≥) 12 43 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 241

Physical properties of grade SUS 304N1-WPA G 4314 (1994)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
194 (≥) 718 (≥) 12 33 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 122
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
754 374 848

Equivalent Products

We can customize the production of SUS 304N1-WPA grade, contact us for the best solution.