SUS 304N2 A Stainless Steels to G 4321 (2000)

SUS 304N2 A - Specification & Application

  • G 4321 (2000) - Stainless steel for building structure

Stainless steel for building structure

Chemical composition(wt.%) of SUS 304N2 A grade: to G 4321 (2000)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn - 2.50
P - 0.045
S - 0.03
Cr 18.00 20.00
Ni 7.50 10.50
N 0.15 0.30
Nb - 0.15

SUS 304N2 A - Detail

Stainless steel for building structure

Mechanical properties of grade SUS 304N2 A G 4321 (2000)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
873 (≥) 619 (≥) 21 14 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 324

Physical properties of grade SUS 304N2 A G 4321 (2000)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
227 (≥) 367 (≥) 43 44 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 112
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
238 276 277

Equivalent Grade

Equivalent Products

We can customize the production of SUS 304N2 A grade, contact us for the best solution.