SUS 430 Stainless Steels to G 4318 (2007)

SUS 430 - Specification & Application

  • G 4318 (2007) - Cold finished stainless steel bars

Cold finished stainless steel bars

Chemical composition(wt.%) of SUS 430 grade: to G 4318 (2007)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.12
Si - 0.75
Mn - 1.00
P - 0.04
S - 0.03
Cr 16.00 18.00
Ni - 0.60
Mo - -
N - -

SUS 430 - Detail

Cold finished stainless steel bars

Mechanical properties of grade SUS 430 G 4318 (2007)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
476 (≥) 485 (≥) 23 34 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 323

Physical properties of grade SUS 430 G 4318 (2007)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
468 (≥) 831 (≥) 42 14 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 433
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
385 742 112