SUS 430TKC Stainless Steels to G 3446 (2012)

SUS 430TKC - Specification & Application

  • G 3446 (2012) - Stainless steel pipes for machine and structural purposes

Stainless steel pipes for machine and structural purposes

Chemical composition(wt.%) of SUS 430TKC grade: to G 3446 (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.12
Si - 0.75
Mn - 1.00
P - 0.04
S - 0.03
Cr 16.00 18.00
Ni - 0.60
Mo - -

SUS 430TKC - Detail

Stainless steel pipes for machine and structural purposes

Mechanical properties of grade SUS 430TKC G 3446 (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
131 (≥) 631 (≥) 31 31 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 324

Physical properties of grade SUS 430TKC G 3446 (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
934 (≥) 591 (≥) 31 23 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 413
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
695 347 856

Equivalent Grade

Equivalent Products

We can customize the production of SUS 430TKC grade, contact us for the best solution.