Stainless steels - Chemical composition
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.09 | ||
Si | - | 0.07 | ||
Mn | - | 1.00 | ||
P | - | 0.040 | ||
S | - | 0.015 | ||
Cr | 16.00 | 18.00 | ||
Ni | 6.50 | 7.80 | ||
Mo | - | - | ||
N | - | - | ||
Al | 0.70 | 1.50 |
Stainless steels - Chemical composition
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
954 (≥) | 216 (≥) | 23 | 12 | 11 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 331 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
791 (≥) | 777 (≥) | 34 | 24 | 31 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 434 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
323 | 637 | 367 |
We can customize the production of X7CrNiAl17-7 grade, contact us for the best solution.