X8Ni9 Stainless Steels to NF EN 10028-4

X8Ni9 - Specification & Application

  • NF EN 10028-4 - Flat products made of steels for pressure purposes - Part 4: Nickel alloy steels with specified low temperature properties
  • NF EN 10222-3 - Steel forgings for pressure purposes - Part 3: Nickel steels with specified low temperature properties
  • NF EN 10269 - Steels and nickel alloys for fasteners with specified elevated and/or low temperature properties

Steels and nickel alloys for fasteners with specified elevated and/or low temperature properties

Chemical composition(wt.%) of X8Ni9 grade: to NF EN 10028-4

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.10
Si - 0.35
Mn 0.30 0.80
P - 0.020
S - 0.010
Cr - -
Ni 8.50 10.00
Mo - 0.10
V - 0.05

X8Ni9 - Detail

Steels and nickel alloys for fasteners with specified elevated and/or low temperature properties

Mechanical properties of grade X8Ni9 NF EN 10028-4

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
363 (≥) 642 (≥) 12 44 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 311

Physical properties of grade X8Ni9 NF EN 10028-4

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
361 (≥) 918 (≥) 34 24 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 233
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
719 587 726

Equivalent Products

We can customize the production of X8Ni9 grade, contact us for the best solution.