Seamless stainless steel tubes for boiler and heat exchanger
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.010 | ||
Si | - | 0.40 | ||
Mn | - | 0.40 | ||
P | - | 0.030 | ||
S | - | 0.020 | ||
Ni | - | 0.60 | ||
Cr | 25.00 | 27.50 | ||
Mo | 0.75 | 1.50 | ||
N | - | 0.015 |
00Cr27Mo
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
594 (≥) | 138 (≥) | 21 | 34 | 42 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 324 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
384 (≥) | 771 (≥) | 13 | 34 | 21 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 323 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
323 | 547 | 216 |
We can customize the production of 00Cr27Mo grade, contact us for the best solution.