Chemical composition(wt.%) of 07X15H7ЮM2 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.05 0.10
Si - 0.70
Mn - 0.70
P - 0.030
S - 0.020
Cr 14.20 15.80
Ni 7.00 8.50
Mo 1.60 2.40
N 0.08 0.18
Ca - 0.10
Mg - 0.10
Ce - 0.10
B - 0.0030

07X15H7ЮM2 - Detail

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Mechanical properties of grade 07X15H7ЮM2

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
775 (≥) 646 (≥) 33 31 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 322

Physical properties of grade 07X15H7ЮM2

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
335 (≥) 875 (≥) 14 31 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 414
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
542 937 922