Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.07 | ||
Si | - | 1.00 | ||
Mn | - | 2.00 | ||
P | - | 0.035 | ||
S | - | 0.020 | ||
Cr | 16.50 | 18.50 | ||
Ni | 19.00 | 21.00 | ||
Mo | 2.00 | 3.00 | ||
Ti | 4×C% | 0.70 | ||
Cu | - | 2.20 |
Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
612 (≥) | 761 (≥) | 24 | 32 | 44 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 332 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
594 (≥) | 971 (≥) | 44 | 31 | 44 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 333 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
394 | 894 | 745 |
We can customize the production of 07X17H20M2Д2T grade, contact us for the best solution.