Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.08 | ||
Si | - | 0.80 | ||
Mn | 7.00 | 9.00 | ||
P | - | 0.035 | ||
S | - | 0.025 | ||
Cr | 15.00 | 17.00 | ||
Ni | - | 0.60 | ||
Mo | 1.80 | 2.50 | ||
N | 0.15 | 0.25 | ||
B | - | 0.002 | ||
Zr | - | 0.10 |
Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
462 (≥) | 375 (≥) | 41 | 24 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 442 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
491 (≥) | 317 (≥) | 14 | 21 | 44 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 223 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
619 | 756 | 755 |
We can customize the production of 08X16Γ8AM2 grade, contact us for the best solution.