Non magnetizable steels. Technical delivery conditions,Ship building,Electrical engineering,Machine engineering,Resistant in sea water up to approx. 60 °C, also against stress corrosion cracking
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|
Non magnetizable steels. Technical delivery conditions
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
811 (≥) | 963 (≥) | 24 | 14 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 411 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
429 (≥) | 665 (≥) | 41 | 21 | 41 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 114 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
315 | 132 | 161 |
We can customize the production of 1-3974 / F49 / S33228 / X2CrNiMnMoNNb23-17-6-3 grade, contact us for the best solution.
–sales@specificsteel.com