10X13Γ18Д Stainless Steels

10X13Γ18Д - Specification & Application

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Chemical composition(wt.%) of 10X13Γ18Д grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.08 0.12
Si - 0.70
Mn 17.00 18.50
P - 0.035
S - 0.030
Cr 12.50 14.00
Ni - 0.90
Mo - 0.30

10X13Γ18Д - Detail

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Mechanical properties of grade 10X13Γ18Д

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
628 (≥) 335 (≥) 42 12 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 131

Physical properties of grade 10X13Γ18Д

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
634 (≥) 586 (≥) 11 23 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 124
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
475 811 933

Equivalent Grade

Equivalent Products

We can customize the production of 10X13Γ18Д grade, contact us for the best solution.