Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.20 | 0.26 | ||
Si | - | 0.60 | ||
Mn | - | 0.60 | ||
P | - | 0.030 | ||
S | - | 0.030 | ||
Cr | 12.00 | 13.50 | ||
Ni | 2.00 | 2.60 | ||
Mo | - | - |
Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
362 (≥) | 668 (≥) | 44 | 32 | 34 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 134 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
284 (≥) | 519 (≥) | 33 | 11 | 11 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 133 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
485 | 652 | 764 |
We can customize the production of 25X13H2BMΦ grade, contact us for the best solution.