Seamless stainless steel tubes for boiler and heat exchanger
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.25 | ||
Si | - | 1.50 | ||
Mn | - | 2.00 | ||
P | - | 0.35 | ||
S | - | 0.03 | ||
Ni | 19.00 | 22.00 | ||
Cr | 24.00 | 26.00 |
2Cr25Ni20
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
813 (≥) | 176 (≥) | 34 | 31 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 442 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
695 (≥) | 839 (≥) | 12 | 22 | 42 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 142 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
963 | 377 | 974 |
We can customize the production of 2Cr25Ni20 grade, contact us for the best solution.
–sales@specificsteel.com