317L Stainless Steels to SAE J 405 (1998)

317L - Specification & Application

  • SAE J 405 (1998) - Chemical compositions of SAE wrought stainless steels

Chemical compositions of SAE wrought stainless steels

Chemical composition(wt.%) of 317L grade: to SAE J 405 (1998)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.03
Cr 18.00 20.00
Ni 11.00 15.00
Mo 3.00 4.00
N - 0.10

317L - Detail

Chemical compositions of SAE wrought stainless steels

Mechanical properties of grade 317L SAE J 405 (1998)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
875 (≥) 394 (≥) 22 31 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 111

Physical properties of grade 317L SAE J 405 (1998)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
678 (≥) 493 (≥) 23 14 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 341
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
958 114 864