Alloyed SiCr steel
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.85 | 0.95 | ||
Si | 1.05 | 1.25 | ||
Mn | 0.60 | 0.80 | ||
P | - | 0.035 | ||
S | - | 0.035 | ||
Cr | 1.10 | 1.30 | ||
Mo | - | - | ||
V | - | - |
Alloyed SiCr steel
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
446 (≥) | 456 (≥) | 12 | 44 | 43 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 441 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
135 (≥) | 656 (≥) | 34 | 42 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 413 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
762 | 317 | 632 |
We can customize the production of 90CrSi5 grade, contact us for the best solution.