Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.15 | ||
Si | - | 1.00 | ||
Mn | 7.50 | 10.0 | ||
P | - | 0.06 | ||
S | - | 0.03 | ||
Cr | 17.0 | 19.0 | ||
Ni | 4.00 | 6.00 | ||
N | - | 0.25 |
ASTM 202
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
981 (≥) | 789 (≥) | 24 | 23 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 131 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
966 (≥) | 626 (≥) | 32 | 42 | 31 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 341 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
989 | 654 | 289 |
We can customize the production of ASTM 202 grade, contact us for the best solution.