Nickel-base superalloy
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.04 | 0.10 | ||
Cr | 18.0 | 21.0 | ||
Ni | - | Remainder | ||
Co | - | 2.0 | ||
Al | 1.0 | 1.8 | ||
Ti | 1.8 | 2.7 | ||
B | - | 0.008 | ||
Fe | - | 1.5 |
GH4180
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
752 (≥) | 387 (≥) | 14 | 24 | 21 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 342 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
856 (≥) | 371 (≥) | 33 | 32 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 331 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
195 | 466 | 693 |
We can customize the production of GH4180 grade, contact us for the best solution.