Specification for Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.20 | ||
Mn | - | 0.80 | ||
Si | - | 3.50 | ||
P | - | - | ||
S | - | - | ||
Cr | - | 18.50 | ||
Ni | - | 14.50 | ||
Mo | - | - | ||
Al | - | 1.00 | ||
N | 0.14 | 0.20 |
Specification for Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
315 (≥) | 757 (≥) | 11 | 21 | 22 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 234 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
179 (≥) | 846 (≥) | 43 | 13 | 34 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 133 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
789 | 544 | 537 |
We can customize the production of SA-213 S30615 grade, contact us for the best solution.