STR35 Stainless Steels to D 3731 (2002)

STR35 - Specification & Application

  • D 3731 (2002) - Heat - resisting steel bars

Heat - resisting steel bars

Chemical composition(wt.%) of STR35 grade: to D 3731 (2002)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.48 0.58
Si - 0.35
Mn 8.00 10.00
P - 0.040
S - 0.030
Cr 20.00 22.00
Ni 3.25 4.50
Mo - -
N 0.35 0.50

STR35 - Detail

Heat - resisting steel bars

Mechanical properties of grade STR35 D 3731 (2002)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
627 (≥) 856 (≥) 14 41 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 232

Physical properties of grade STR35 D 3731 (2002)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
749 (≥) 432 (≥) 31 23 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 441
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
631 146 123

Equivalent Grade

Equivalent Products

We can customize the production of STR35 grade, contact us for the best solution.