STS305WSA Stainless Steels to D 3697 (2002)

STS305WSA - Specification & Application

  • D 3697 (2002) - Stainless steel wires for cold heading and cold forging

Stainless steel wires for cold heading and cold forging

Chemical composition(wt.%) of STS305WSA grade: to D 3697 (2002)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.12
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.030
Cr 17.00 19.00
Ni 10.50 13.00
Mo - -
N - -

STS305WSA - Detail

Stainless steel wires for cold heading and cold forging

Mechanical properties of grade STS305WSA D 3697 (2002)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
613 (≥) 259 (≥) 42 31 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 241

Physical properties of grade STS305WSA D 3697 (2002)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
284 (≥) 747 (≥) 42 14 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 434
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
927 481 982