STS430F Stainless Steels to D 3692 (2001)

STS430F - Specification & Application

  • D 3692 (2001) - Cold finished stainless steel bars
  • D 3702 (2008) - Stainless steel wire rods
  • D 3703 (2007) - Stainless steel wires
  • D 3706 (2008) - Stainless steel bars
  • D 7202 (2004) - Free - machining stainless steel wire and wire rods

Free - machining stainless steel wire and wire rods

Chemical composition(wt.%) of STS430F grade: to D 3692 (2001)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.12
Si - 1.00
Mn - 1.25
P - 0.060
S - 0.15
Cr 16.00 18.00
Ni - 0.60
Mo - -
N - -

STS430F - Detail

Free - machining stainless steel wire and wire rods

Mechanical properties of grade STS430F D 3692 (2001)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
726 (≥) 925 (≥) 33 13 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 243

Physical properties of grade STS430F D 3692 (2001)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
582 (≥) 988 (≥) 22 12 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 422
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
552 329 371

Equivalent Products

We can customize the production of STS430F grade, contact us for the best solution.
sales@specificsteel.com